MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LG Chemical Non-Aromatic Raffinate
Categories: Fluid

Material Notes: Structure & Characteristics: Produced as a by-product of aromatics extraction process, and is mainly composed of non-aromatics of C6~C8.

Uses: Used to blend solvent or gasoline.

CAS: 78-78-4, 109-66-0, 110-54-3, 96-37-7 and 109-66-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.749 g/cc0.749 g/cc
Molecular Weight 84.2 g/mol84.2 g/mol
Vapor Pressure 0.0693 bar
@Temperature 20.0 °C
52.0 torr
@Temperature 68.0 °F
Vapor Density=2.9
 
Thermal PropertiesMetricEnglishComments
Melting Point -142.4 °C-224.3 °F
Boiling Point 71.8 °C161 °F
Flash Point -4.00 °C24.8 °F
Ignition Temperature 315 °C599 °FAutoignition
 
Descriptive Properties
Components2,2-Dimethy-butane0.01%
 2,3-Dimethyl –2-butene0.04%
 2,3-Dimethyl-pentane0.09%
 2-Methyl-pentane9.2%
 3-methyl-pentane4
 Benzene<0.2%
 Cyclohexane7.8%
 cyclo-Pentane5.5%
 iso-Heptane1.5%
 iso-Octane1.7%
 Iso-Pentane0.7%
 Methylcyclohexane5%
 Methylcyclopentane31.9%
 n-Heptane2.83%
 n-Hexane13.3%
 n-Octane0.45%
 n-Pentane0.6%
 Other15.38%
 Total Sulfur<100 ppm, ASTM D5453

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLAY761 / 148771

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.