MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis Clearflex® DFH 20 Film Grade LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Clearflex® DFH 20 is a Linear Low Density Polyethylene Resin butene comonomer produced by Unipol gas phase technology. Clearflex® DFH 20 exhibits a typical wide molecular weights distribution which gives an excellent process ability together with good mechanical characteristics. Application: Clearflex® DFH 20 is mainly designed for the production of micro-irrigation tubes, durable hoses and pipes, extruded profiles and for the production by injection molding of fittings. The outdoor use, requires the with anti-UV, to maintain excellent performance even after prolonged periods of exposure to sunlight.

Property data reported for compression molded specimens.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ISO 1183
Environmental Stress Crack Resistance >= 500 hour>= 500 hourCompression Molded; ASTM D 1693(B)
Melt Flow  0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 44 g/10 min
@Load 21.6 kg,
Temperature 190 °C
44 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444Compression Molded; ISO 868 A
Tensile Strength at Break 15.0 MPa2180 psiISO 527-3
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiISO 527-3
Tensile Strength, Yield 11.0 MPa1600 psiISO 527-3
Elongation at Break >= 800 %>= 800 %ISO 527-3
Flexural Modulus 0.310 GPa45.0 ksiISO 178
1% Secant Modulus, MD 140 MPa20300 psiISO 527-3
1% Secant Modulus, TD 140 MPa20300 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 120 °C248 °FManufacturer method
Vicat Softening Point 110 °C
@Load 1.00 kg
230 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D 746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FAs Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9825 / 265529

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.