NABALOX® aluminum oxide has a number of advantages including - low sintering temperature
- wide sintering range
- flexible processing
- high sintered densities high wear and impact resistance
- electrical insulation
- high mechanical strength
- high temperature properties
- dimensional accuracy
- optimized chemical resistance
Chemical industry, Glass industry, Corundum, Refractory industry, Household ceramics, Electroceramics, Engineering ceramics Information provided by Nabaltec. |