MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Eastman Advantis™ 550-1 25X adhesion promoter
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eastman Advantis™ 550-1 25X adhesion promoter is a nonchlorinated product for adhesion to TPO and polypropylene-based substrates. Nonchlorinated systems are known to demonstrate excellent performance under 2-part urethane (2K) coatings, but often their application is limited to 2Ks. Advantis 550-1 25X expands nonchlorinated performance to applications under many melamine-cured systems. Formulators can expect a boost in gasoline resistance performance by adding Advantis 550-1 25X to their current adhesion promoter system. Due to its lack of chlorine and its chemical structure, Advantis 550-1 25X exhibits excellent humidity and gasoline resistance, particularly under 1K systems. Advantis 550-1 25X adhesion promoter is available at 25% weight solids in aromatic 100 or in xylene. If the solution gels due to storage at low temperatures, it can be re-liquefied by warming with agitation.

Applications

  • Auto omen
  • Auto plastics
  • Auto refinish
  • Automotive
  • Automotive parts & accessories
  • Consumer electronics
  • General industrial coatings
  • Graphic arts
  • Truck/bus/rv
Key Attributes
  • Excellent gasoline resistance

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 1.00 g/cc<= 0.0361 lb/in³
 
Thermal PropertiesMetricEnglishComments
Boiling Point 137 - 144 °C279 - 291 °F
Decomposition Temperature 500 °C932 °FNo exotherm to
Flash Point 27.0 °C80.6 °FPensky-Martens Closed Cup
 
Descriptive Properties
Appearanceviscous liquid
Coloryellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4012 / 323635

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.