MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco Cepheus® 220
Categories: Fluid; Lubricant

Material Notes: Texaco Cepheus oil deliver value through
  • The ability to retain lubrication properties in the presence of water.
  • Good rust protection from a carefully designed additive package.
  • The ease with which they can be washed off textiles

Texaco Cepheus oils are naphthenic based oils compounded with fatty oils. They protect well against rusting and feed line plugging.

Texaco Cepheus oils are suitable for lubricating bearings and other machine parts of textile machines are well as other industrial equipment needing lightly compounded lubricants

Texaco Cepheus 150 and 220 are recommended for air compressor applications where there is the possibility of carbon buildup or where there is significant moisture.

Do not use in breathing air apparatus or medical equipment.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222777; MSDS Number: 8958

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 20.5 °20.5 °
Viscosity Measurement 1010Viscosity Index
Saybolt Viscosity at 100°F 1135 SUS1135 SUS
Saybolt Viscosity at 210°F 70.3 SUS70.3 SUS
Kinematic Viscosity at 40°C (104°F) 209 cSt209 cSt
Kinematic Viscosity at 100°C (212°F) 12.6 cSt12.6 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -20.0 °C-4.00 °F
Flash Point 218 °C424 °F
 
Descriptive Properties
Fatty Oil wt %3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA044 / 76923

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.