MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds SMASH!® Plastic Breakaway Glass Plastic
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: SMASH! Plastic™ is a urethane liquid plastic designed to shatter/crumble on impact (“breakaway glass”). SMASH! Plastic™ is water clear and, once fully cured, shatters like glass. It can be cast solid in thin sections to make window panes or rotationally cast to form hollow bottles, jars or other glass-like objects to be used as breakable props for movie and stage productions. Maximum recommended thickness is 1/8” (0.33 cm.). SMASH! Plastic™ is a room temperature cure system that is easy to use – mixed 1A:1B by volume (1 cup + 1 cup). Low viscosity ensures easy mixing and pouring. Cured castings are UV RESISTANT. Vibrant colors and color effects are achieved by adding pigment dispersions.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.036 g/cc1.036 g/ccASTM D-1475
Viscosity 900 cP900 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.00010 cm/cm0.00010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D-2240
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 min1.50 hourHandling Time
Pot Life 5.00 min5.00 minASTM D-2471
 
Descriptive Properties
ColorClear
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume26.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN048 / 296749

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.