This layer combines the advantages of Duplex-TiCN and FORMATIC®. The new DUMATIC layer is always manufactured as a Duplex version, therefore with a plasma diffusion process of the base material. The layer itself has a structured multi-layer design with high content of TiC (approx. 4000 HV! ). The uppermost layer is developed as slide-favorable and colored sealing coat.Information provided by Eifeler Coatings Technology |