MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin PKN4775 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PKN4775 resin is a non-reinforced, opaque blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high heat, thin wall extrusion and injection moldable grade is an improved version of NORYL PKN4736 resin and exhibits modulus at elevated temperature and good chemical resistance. NORYL PKN4775 resin is an excellent candidate for applications in high performance packaging. *See NORYL PKN4775F resin for FDA food compliant version.

Features: Low Creep Sensitivity,High Heat Resistance,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Moisture Absorption 0.000 %0.000 %Sheet Extrusion
 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %0.25 %ISO 62-1
Viscosity 14 cP
@Load 5.00 kg,
Temperature 300 °C
14 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 15.3 g/10 min
@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psi50 mm/min; ASTM D638
 47.0 MPa6820 psi50 mm/min; ISO 527
Tensile Strength, Yield 51.0 MPa7400 psi50 mm/min; ASTM D638
 51.0 MPa7400 psi50 mm/min; ISO 527
Elongation at Break 29.3 %29.3 %50 mm/min; ISO 527
 35 %35 %50 mm/min; ASTM D638
Elongation at Yield 4.1 %4.1 %50 mm/min; ISO 527
 5.1 %5.1 %50 mm/min; ASTM D638
Tensile Modulus 2.12 GPa307 ksi5 mm/min; ASTM D638
 2.12 GPa307 ksi1 mm/min; ISO 527
Flexural Strength 78.0 MPa11300 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 82.0 MPa11900 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.16 GPa313 ksi2 mm/min; ISO 178
 2.21 GPa321 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 268 J198 ft-lbASTM D256
 161 J
@Temperature -30.0 °C
119 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 39.0 J28.8 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  92.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 92.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 3.20 mm
280 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
252 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 142 °C288 °FRate B/50; ASTM D1525
 142 °C288 °FRate B/50; ISO 306
 144 °C291 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Zone 1 205 - 225 °C401 - 437 °FSheet Extrusion
Zone 2 215 - 240 °C419 - 464 °FSheet Extrusion
Zone 3 240 - 265 °C464 - 509 °FSheet Extrusion
Zone 4 240 - 265 °C464 - 509 °FSheet Extrusion
Adapter Temperature 240 - 265 °C464 - 509 °FSheet Extrusion
Die Temperature 240 - 265 °C464 - 509 °FSheet Extrusion
Melt Temperature 265 - 275 °C509 - 527 °FSheet Extrusion
Roll Temperature 105 - 120 °C221 - 248 °FRoll Stack Temp - Bottom
 105 - 120 °C221 - 248 °FRoll Stack Temp - Middle
 105 - 120 °C221 - 248 °FRoll Stack Temp - Top
Drying Temperature 70.0 - 80.0 °C158 - 176 °FSheet Extrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourSheet Extrusion
 8.00 hour8.00 hourCumulative; Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82420 / 290367

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.