MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cookson Group POLYSOLDER® LT One Part Electrically Conductive Adhesive Paste  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: This material is a lead-free, no clean, environmentally acceptable solder substitute specifically designed for electronic component assembly, especially surface mount. This product is can be screen printed, stenciled or pneumatically dispensed as a thixotropic paste. The material is hardened by thermal processing in IR, convection, conduction or vapor phase equipment. This patented product is a unique electronics polymer material that forms stable electrical and mechanical junctions with standard components, even after extended environmental aging.

Features:

  • Pb-Free
  • Intrinsically Clean
  • Fine Pitch
  • Low Stress
  • Stable Junctions
  • Removable

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 78 - 82 %
Viscosity 150000 cP
@Temperature 25.0 °C
HBT 5x cp-51 spindle, 1 rpm
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength >= 2500 psiDie shear
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00050 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 54.0 µm/m-°CBelow Tg
Thermal Conductivity 3.50 W/m-K
Glass Transition Temp, Tg 90.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 480 - 720 minOn screen
Shelf Life 6.00 Month
@Temperature -40.0 °C
 
Descriptive Properties
Assembly Temperature130-170°C
Junction Resistivity<25 mohmTypical, tin-lead coated components
Push Off Strength13-15 lbs1206 chip resistor
 35-40 lbs68PLCC quad pack, 50 mil pitch

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLASK089 / 56379

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.