MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik DYNACOLL® S 1272 Copolyester
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Copolyesters: With its DYNACOLL® S product range Evonik offers thermoplastic copolyesters of high molecular weight to a wide variety of thermoplastic hot melt and solvent based applications. The individual grades differ in their melting point, degree of crystallinity and hardness and in their setting time. According to their crystallinity, the product range is arranged into four basic groups:
  • DYNACOLL® S - Highly crystalline grades
  • DYNACOLL® S - Moderately crystalline grades
  • DYNACOLL® S - Slightly crystalline grades
  • DYNACOLL® S - Amorphous grades
DYNACOLL® S copolyesters are generally supplied as granules, usually in bags of 20 or 25 kg. They can be processed into following forms of applications: adhesive film, web or net, powder, paste, hot melt and solution.

Your benefits: DYNACOLL® S - Moderately crystalline grades

  • moderate open times
  • very good adhesive strength and heat resistance

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  65 cP
@Temperature 200 °C
65 cP
@Temperature 392 °F
DIN EN ISO 3219
 140 cP
@Temperature 180 °C
140 cP
@Temperature 356 °F
DIN EN ISO 3219
 320 cP
@Temperature 160 °C
320 cP
@Temperature 320 °F
DIN EN ISO 3219
Viscosity Number 84 cm³/g0.84 dl/gDIN 53728
Melt Flow  30 g/10 min
@Load 2.20 kg,
Temperature 160 °C
30 g/10 min
@Load 4.85 lb,
Temperature 320 °F
DIN ISO 1133
 60 g/10 min
@Load 2.20 kg,
Temperature 180 °C
60 g/10 min
@Load 4.85 lb,
Temperature 356 °F
DIN ISO 1133
 120 g/10 min
@Load 2.20 kg,
Temperature 200 °C
120 g/10 min
@Load 4.85 lb,
Temperature 392 °F
DIN ISO 1133
 250 g/10 min
@Load 2.20 kg,
Temperature 220 °C
250 g/10 min
@Load 4.85 lb,
Temperature 428 °F
DIN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353DIN 53505
Tensile Strength at Break 25.0 MPa3630 psiDIN EN ISO 527-1/3
Elongation at Break 400 %400 %DIN EN ISO 527-1/3
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °FDIN 53765
Softening Point 140 °C284 °FDIN ISO 4625
Glass Transition Temp, Tg 0.000 °C32.0 °FDIN 53765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL090 / 196294

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.