MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Fast cycling, broad temperature performance, and durability

Uses: Injection Molding

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inflex bar
 0.0090 cm/cm0.0090 in/indisk
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 87 - 93
@Time 5.00 sec
87 - 93
@Time 0.00139 hour
ASTM D2240
Tensile Strength 33.0 MPa4790 psiASTM D412
Elongation at Break 645 %645 %ASTM D412
100% Modulus 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
ASTM D412
300% Modulus 17.0 MPa
@Strain 300 %
2470 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0386 GPa5.60 ksiASTM D790
Tear Strength 29.8 kN/m170 pliTrouser; ASTM D470
Graves Tear Strength 116 kN/m660 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4545CS-17, 1000g; ASTM D3389 B
 
Thermal PropertiesMetricEnglishComments
Melting Point 179 °C354 °FDSC
Glass Transition Temp, Tg -47.0 °C-52.6 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 200 °C392 °FInjection
Middle Barrel Temperature 204 °C399 °FInjection
Front Barrel Temperature 210 °C410 °FInjection
Nozzle Temperature 215 °C419 °FInjection
Melt Temperature 215 °C419 °FInjection
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiInjection
Hold Pressure 34.5 - 68.9 MPa5000 - 10000 psiInjection
Back Pressure >= 0.345 MPa>= 50.0 psiInjection
Screw Speed 60 - 100 rpm60 - 100 rpmInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane

PNOVEON022 / 55288

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.