ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It has been formulated for excellent antistatic properties.
ATOFINA Propylene PPC 12712 has been developed for high speed injection molding of thin walled packaging containers and household articles. Information provided provided by Total Petrochemicals. Total Petrochemicals acquired former Fina and Atofina plastics product lines. |