MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® Michem® Guard 1350 Nonionic emulsion of polyethylene wax
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Nonionic emulsion of polyethylene wax

Usage: Michem® Guard 1350 is a water based one micron dispersion which improves rub and abrasion resistance in pigmented coatings and semi-gloss coatings, inks and OPVs at very low addition rates. Addition of Michem® Guard 1350 has little effect on gloss.

Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooring

Food Contact Information when manufactured in the USA:
FDA:
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 1.00 g/cc0.980 - 1.00 g/cc
Volatiles 49.5 - 50.5 %49.5 - 50.5 %
pH 4.0 - 104.0 - 10Recommended pH of system
 7.0 - 8.07.0 - 8.0
Brookfield Viscosity <= 500 cP<= 500 cPSpindle # 2, rpm 60
 
Descriptive Properties
AppearanceWhite liquid
Emulsifier ChargeNonionic
Solids TypePolyethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOWAX® X 4118 Polyethylene Wax
Evonik VESTOWAX® AW 1060 Polyethylene Wax
Evonik VESTOWAX® AS 1550 Polyethylene Wax
Evonik VESTOWAX® AS 1550 E Polyethylene Wax
Evonik VESTOWAX® AO 3533 Polyethylene Wax

WMICHEL126 / 135043

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.