MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 11044DB Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 11000 series are engineered low friction slip coating materials designed primarily for demanding automotive and industrial applications. This product is a high hardness, low density grade with good UV resistance and superior abrasion resistance are co-extruded with TPE-S, TPE-V and EPDM.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Bondability; Chemical Resistant; Good Adhesion; Good Processability; High Hardness; High Heat Resistance; Low Compression Set; Low Density; Low Friction; Low Specific Gravity; Specialty Grade; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Coating Applications; Industrial Applications; Rubber Replacement; Weatherstripping

RoHS Compliance: RoHS Compliant

Automotive Specifications: DAIMLER DBL 5578 Color: Black; NISSAN Unspecified Color: Black; VAG VW501 23 Color: Black; VAG VW501 2G Color: Black

Form: Pellets

Processing Method: Coextrusion; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Viscosity 312 cP
@Shear Rate 206 1/s,
Temperature 200 °C
312 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 40
@Time 5.00 sec
40
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 11.0 MPa1600 psiAcross Flow; ISO 37
Elongation at Break 550 %550 %Across Flow; ISO 37
Tensile Modulus 0.173 GPa25.1 ksiISO 178
Coefficient of Friction 0.250.25vs Glass - Dynamic; ASTM D1894
 
Processing PropertiesMetricEnglishComments
Zone 1 177 - 210 °C350 - 410 °F
Zone 2 182 - 216 °C360 - 420 °F
Zone 3 193 - 227 °C380 - 440 °F
Zone 4 193 - 227 °C380 - 440 °F
Zone 5 193 - 227 °C380 - 440 °F
Die Temperature 193 - 227 °C380 - 440 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase TPSiV® 1180-50D Thermoplastic Silicone Vulcanizate
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer
Celanese SO.F.TER Sofprene® Vulcanized Rubber 38 KH SBS Foot Ware Compound

PTEKNQ1227 / 237718

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.