MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Duomeen CD Coco propylene diamine
Categories: Other Engineering Material

Material Notes: Duomeen CD is a coco propylene diamine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.796 g/cc
@Temperature 80.0 °C
0.0288 lb/in³
@Temperature 176 °F
 0.803 g/cc
@Temperature 70.0 °C
0.0290 lb/in³
@Temperature 158 °F
 0.810 g/cc
@Temperature 60.0 °C
0.0293 lb/in³
@Temperature 140 °F
 0.824 g/cc
@Temperature 40.0 °C
0.0298 lb/in³
@Temperature 104 °F
 0.836 g/cc
@Temperature 25.0 °C
0.0302 lb/in³
@Temperature 77.0 °F
pH <= 10<= 10
Viscosity 58 cP58 cP
Vapor Pressure 0.000130 bar0.0975 torr
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  2.49 J/g-°C
@Temperature 37.8 °C
0.595 BTU/lb-°F
@Temperature 100 °F
 2.56 J/g-°C
@Temperature 60.0 °C
0.612 BTU/lb-°F
@Temperature 140 °F
Melting Point 15.0 °C59.0 °F
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
>= 572 °F
@Pressure 14.6921 psi
Pour Point 21.0 °C69.8 °F
Flash Point >= 150 °C>= 302 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 2.00.00 - 2.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 2.0 %<= 2.0 %
 
Descriptive Properties
Amine number409-442 mg KOH/g
AppearanceLiquid
Cloud point23°C
Content= 45 %Primary Amine
 = 45 %Secondary Amine
 0-12 g I2/100 gIodine value
 127-137 g/eqNeutralization equivalent
Equivalent mass132 g/eq
HLB17.5Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY491 / 286014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.