MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ 741 A/B Epoxy Adhesive System
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Thermoset 741 A/B is a medium viscosity, high strength, epoxy structural adhesive featuring rapid cure in thin films and a convenient mix ratio by volume. This material cures to a tough, high impact polymer, and provides exceptional adhesion to a wide variety of substrates. 741 A/B can also be used in small potting applications where minimal flow during cure is desired.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.57 lb/galPart B
 10.02 lb/galPart A
Viscosity 30000 cP
@Temperature 25.0 °C
Part B
 50000 cP
@Temperature 25.0 °C
Part A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80cured
Tensile Strength 7800 psiCured
Elongation at Break 3.5 %cured
Compressive Strength 9800 psicured
Shear Strength 2000 psiTensile (AI/AI), cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
Dielectric Constant 4.3
@Frequency 1000 Hz
Dielectric Strength 450 V/mil
Dissipation Factor 0.034
@Frequency 1000 Hz
 
Processing PropertiesOriginal ValueComments
Pot Life 3.00 - 5.00 min
@Temperature 25.0 °C
in a 20 gram mass
 
Descriptive Properties
AppearanceLight Amber SyrupPart B
 Translucent SyrupPart A
Mix Ratio1 part 741 A to 1 part 741 Bby volume
 1 part 741 A to 96 parts 741 Bby weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9154 / 232542

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.