MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Techmer ES Electrablend® PPS 06001
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler; Polyphenylene Sulfide (PPS), Conductive

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Carbon Fiber Reinforcement

Features: Electrically Conductive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ASTM D2240
Tensile Strength at Break 9800 psiASTM D638
Elongation at Break 100 %ASTM D638
Flexural Modulus 80000 psiASTM D790
Tear Strength 200 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 - 1000 ohm-cmASTM D257
Surface Resistance 10 - 1000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 220 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES Electrafil® J-1/CF/40 NAT PA66
Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled
Techmer ES Electrablend® PA6 04001 BK MB Glass/Stainless Steel Filled
Techmer ES Electrablend® PA12 Stainless Steel Filled
Techmer ES Electrablend® PA12 CB

PTPC1044 / 136982

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.