MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lushan PR-2A Maleic Anhydride Grafted Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Malic anhydride grafted polypropylene (PP-a-MAH) Lushan series is evaluated as compatiblizer/coupling agent which is used to fill or reinforced polypropylene. As the coupling agent, PP-g-MAH can significantly improve the filled or enhanced PP’s mechanical properties and heat resistance. As the same time, the introduction of introduction of polypropylene molecular chain polar groups could significantly improve PP’s shading ability.

Maleic Anhydride Grafted Polypropylene Usage:

  • As compatibilizer/ coupling agent for polypropylene filled with glass fiber or mineral: maleic anhydride grafted polypropylene as a high polarity. As long as adding a small amount (4%), it can significantly improve interface bonding strength between PP and the glass fiber, talc; mica and other inorganic fillers. Modified polypropylene’s tensile strength, bending strength and impact strength have been improved significantly.
  • As compatibilizer/coupling agent for PA/PP, PA/PE alloy: to improve the processing of nylon, impact resistance, lower water absorption and products dimensional stability.
  • Improve coating and painting/shagging properties for polypropylene.

    Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Index of Compound 80 g/10 min80 g/10 min
 
Descriptive Properties
AppearanceNatural color of light yellow granule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lushan PR-3 Maleic Anhydride Grafted Polypropylene
Polyram Bondyram® 1010 Maleic Anhydride Modified Polypropylene
Polyram Bondyram® 1101 Maleic Anhydride Modified Homo Propylene
Polyram Bondyram® 1004 Maleic Anhydride Modified Homo-Polypropylene
Polyram BondyRam® 1001 Maleic Anhydride modified Homo-polypropylene coupling agent

PLUSH047 / 150045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.