MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANMELTTHANE® PES-690-G Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANMELTTHANE® PES-690-G is a saturated co polyester. It is specially used as a hot-melt adhesive for filter bonding. DANMELTTHANE® PES-690-G distinguishes itself by an extremely high melting point and a high melting viscosity for the bonding of filters. Films of DANMELTTHANE® PES-690-G are flexible and break resistant. When cutting the bonded filter elements there is no smearing and the tools are not contaminated by the glue line of DANMELTTHANE ® PES-690-G.

Application: DANMELTTHANE® PES-690-G makes it possible to do the folding and the joining of filter-web papers before and/or after the impregnation with phenol resin and/or the polymerization. The polymerization temperature is supposed to be between 180 and 185 °C. DANMELTTHANE® PES-690-G is qualified for the bonding of automobile-, air-, industrial-, household-, protection-, dirt-, dust- and medical filters.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Brookfield Viscosity 30000 - 40000 cP
@Temperature 232 °C
30000 - 40000 cP
@Temperature 450 °F
RVT
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 - 180 °C338 - 356 °FDSC 20 °C / min
 210 - 220 °C410 - 428 °FKOFLER
Ring & Ball Softening Point 170 - 172 °C338 - 342 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 260 °C428 - 500 °F
Moisture Content <= 0.10 %<= 0.10 %
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectGranules
Open time<10 sec
Polymerization temperature<185°Cduring the at process of filter production
TypeSaturated thermoplastic polyester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ126 / 294546

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.