MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

GEHR Plastics PA 6 Nylon 6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing. In addition, this conditioning occurs with a longer storage in air automatically.

Properties:

  • high impact strength and stiffness
  • high impact and notching impact strength
  • high heat deflection temperature
  • good at dampening
  • good glide and limp home characters
  • good chemical stability against organic solvents and fuels
  • size alteration by humidity absorption must be considered
  • dimension stability, electrical and mechanical properties may become affected by absorbing moisture or water
Applications include bearing parts, gear wheels, pump parts, sliding rails, castors, and fittings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccISO 1183
Water Absorption 9.5 %9.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
Elongation at Yield 20 %20 %ISO 527
Modulus of Elasticity 1.00 GPa145 ksiISO 527
Charpy Impact, Notched NBNBISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+10 ohm-cm>= 1.00e+10 ohm-cmVDE 0303
Surface Resistivity per Square >= 1.00e+10 ohm>= 1.00e+10 ohmVDE 0303
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
DIN 53483
Dielectric Loss Index 0.30
@Frequency 1e+6 Hz
0.30
@Frequency 1e+6 Hz
DIN 53483
 
Descriptive Properties
Aromatic Resistancelimited
ColorNatural
Hydrocarbonate Resistancelimited
Ketone Resistancelimited
Resistance Against Hot Waterlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGEHR017 / 79854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.