MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ovako 38MnVS6 482A Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Grade 38MnVS6 is a micro-alloyed medium carbon steel for general purposes. The steel is recommended for applications demanding high mechanical properties and smooth surfaces.
482A - Ingot cast variant
7221 - Continuous cast variant.
SB9857 - Continuous cast variant.

Information provided by Ovako

Key Words: SB9857 - 39MnV5, Ovako482A, 482, SB482, Imatra482
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 300
@Thickness 90.0 - 140 mm
Round bar
Tensile Strength 850 - 1000 MPa
@Thickness 90.0 - 140 mm
Round bar
Tensile Strength, Yield >= 580 MPa
@Thickness 90.0 - 140 mm
Reh, Round bar
Elongation at Break 14 %
@Thickness 90.0 - 140 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 20.0 J
@Thickness 90.0 - 140 mm,
Temperature 20.0 °C
Round bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 330 °CMS
 720 °CAC1
 780 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.37 - 0.40 %
Chromium, Cr 0.20 - 0.26 %
Iron, Fe 97.12 - 97.55 %As Balance
Manganese, Mn 1.25 - 1.35 %
Molybdenum, Mo <= 0.050 %
Nickel, Ni 0.15 - 0.20 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.35 - 0.42 %
Sulfur, S 0.020 - 0.028 %
Vanadium, V 0.11 - 0.15 %
 
Descriptive Properties
WeldabilityCEV 0.75max
 Pcm 0.53max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako 38MnVS6 SB9857 Steel, +AR
Ovako 38MnVS6 EN 10267:1998 Steel, +AR
Ovako 38MnVS6 7221 Steel, +AR

NOVAKO274 / 234573

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.