MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chengdu Polyster KP-200-30 Silicone Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Silicone

Material Notes: KP-200 series silicone masterbatches are white pellets or white powder which made from ultra-high molecular weight polysiloxane, used by plastics as processing aids and impart expected silicone benefits to plastics, often more efficiently and more effectively than lower molecular weight silicone fluids, such as safety, little effect on the adhesion of paints, labels or decorations, more convenient to handle, good dispersion. Silicone masterbatches are with the carrier of polyethylene. For KP-200-30 silicone masterbatch, the content of siloxane is 30%. For KP-200-40 silicone masterbatch, the content of siloxane is 40%. For KP-200-50 silicone masterbatch, the content of siloxane is 50%. KP-200H silicone masterbatch is 100% pure silicone powder. KP-200 silicone masterbatch is with special silicon powder carrier, the content of silicone with ultra-high molecular weight is 50%.

Information provided by Chengdu Polyster Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
GB/T 3682
 
Component Elements PropertiesMetricEnglishComments
Silicon, Si 33 %33 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 922-LO Silicone
Elkem Silicon Injection Grade
Master Bond MasterSil 970-LO Silicone
Dow 1250 SURFACTANT

PCHEN025 / 79322

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.