MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess LEWATIT® MonoPlus S 108 KR Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus S 108 KR is a strongly acidic, gel-type cation exchange resin with beads of a uniform size (monodisperse), in highly regenerated form (min 99% H) and purified (extremely low content of desorbable chloride ions) to meet nuclear industry specifications. Lewatit nuclear resins (Lewatit KR) are noted for their outstanding mechanical and chemical stability and their high osmotic stability. The high total capacity results in high operation capacities with a very low ionic leakage and a very high regenerant utilization. Because of their excellent hydrodynamic properties, Lewatit KR resins allow particularly high flow rates. The extremely high monodispersity [uniformity coefficient: 1.05 (+/- 0.05)] and very low fines content of max 0.1% (<0.4 mm) results in particularly low pressure losses paired with standard resins. Used in radioactive water circuits, they provide a number of special tasks and guarantee a water quality that fully complies with the requirement of the nuclear power industry. Lewatit MonoPlus S 108 KR is especially suitable for:
  • the removal of cations, including radioactive isotopes, from aqueous solutions (pH control through adsorption of excess)
  • the decontamination of circuits in nuclear reactor plants
  • the removal of radioactive cations such as cesium 137 (fuel cooling)
  • the treatment of primary coolant e.g. in pressure water reactors
  • the purification of steam generator blowdown irrespective of the conditioning with Levoxin (hydrazine), ethanolamine or morpholine
  • the removal of activated cleavage or corrosion products, including mechanical filtration of suspended impurities
  • the polishing in the primary and secondary sections as a mixed bed component with Lewatit MonoPlus M 800 KR or Lewatit MonoPlus MP 800 OH.
Important! Rinse carefully with demineralized water prior to service or mixing with Lewatit MonoPlus M 800 KR or Lewatit MonoPlus MP 800 OH

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.790 g/cc0.0285 lb/in³
Density 1.22 g/cc0.0441 lb/in³
Bead Size 0.600 - 0.700 mm0.0236 - 0.0276 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlack-brown
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8797 / 209189

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.