MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Inov Chem DY3516 90 Shore A, MDI-terminated Polyester system
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE

Material Notes: Description: It is used to produce Polyurethane sieves, PU rollers and other elastomer. It should be processed by mid-temperature casting machine. The final product enjoys good anti resistance ability, good rebound. And the hardness can be adjusted by the different ratio. The color can be adjusted by pigment.

Application: automotive kits, pipe cleaners, etc., polyurethane large or small product components.

Ratio:
DY3516-B: 100
DY3516-A: 60
DY3516-C: 14.5
Catalyst/total amount A+B+C: 0.3%

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 30 cPC
 700 cPB
 730 cPA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
 
Processing PropertiesOriginal ValueComments
Mold Temperature 100 °C
Cure Time 30.0 min
@Temperature 90.0 °C
Open Mold Time
Gel Time 4.00 min
 
Descriptive Properties
NCO content16.3-16.7%B
Operation temperature45°CB
 45°CC
 70°CA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM123 / 312652

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.