MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Universal Wire Works 310 Stainless Steel (AMS 5694) Filler Metal
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Universal 310 alloy is primarily used for welding type 310 stainless steels, dissimilar steels and such types as 405, 410 and 430 steels when preheat and postheat are not practical. This alloy exhibits high temperature tensile strength and resistance to scaling and is often used on heat exchangers, combustion chambers, gas turbine parts and jet engine rings.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 586 MPa85000 psi
Tensile Strength, Yield 379 MPa
@Strain 0.2 %
55000 psi
@Strain 0.2 %
Elongation at Break 35 %35 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %
Chromium, Cr 26.5 %26.5 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe >= 48.8 %>= 48.8 %As Remainder
Manganese, Mn 1.7 %1.7 %
Molybdenum, Mo <= 0.75 %<= 0.75 %
Nickel, Ni 21.2 %21.2 %
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.40 %0.40 %
Sulfur, S 0.010 %0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
310 Stainless Steel, annealed bar
304 Stainless Steel
310 Stainless Steel, annealed sheet
310 Stainless Steel, annealed plate
420 Stainless Steel

NUWW284 / 19728

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.