MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 950 Epoxy Prepreg with Hy-E Std/950 Unidirectional Tape and Roving
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 950 resin is a 250 – 300°F (121 – 149°C) curing epoxy resin with good 220°F (104°C) dry service capability. It can be impregnated via hot melt or solution techniques on all available fibers and fabrics. CYCOM 950 is formulated for shrink tape processing, but it has been successfully processed by autoclave, press molding and vacuum bagging. Unidirectional tape and woven fabric impregnated with CYCOM 950 resin will retain excellent tack and drape for at least 10 days at 72°F (22°C). Standard cure is for 90 minutes at 275°F (135°C). No post cure is required for 220°F (104°C) dry service capability. The recommended autoclave lay-up procedure for this material is L-3 or L-6. The recommended cure procedure is C-6 or C-7 at 275°F (135°C).

Features & Benefits:

  • Available in a broad range of fibers and forms including tape, fabric and roving
  • Self-adhesive
  • Low flow
  • 220°F (104°C) dry and 180°F (82°C) wet service temperature
  • Laminate and sandwich panel usage
  • Multiprocessing capable: shrink tape, autoclave, press mold, vacuum bag
  • Shelf life of 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
Applications: Tubular structures such as fishing rods, golf shafts and bike components

Typical Properties of CYCOM 950 Composite Laminate with Standard Modulus (33 Msi/228 GPa Class) Unidirectional Tape and Roving - CEM Product Code Hy-E Std/950

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 290000 - 320000 psi
Elongation at Break 1.3 - 1.6 %
Tensile Modulus 131 - 145 GPa
Flexural Strength 230000 - 265000 psi
Flexural Modulus 117 - 138 GPa
Compressive Strength 179 - 207 MPaAfter impact
 1172 - 1517 MPa
Compressive Modulus 103000 - 117000 MPa
Shear Strength 14000 - 16000 psiShort Beam
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °Cwet
 104 °Cdry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 300 °FStandard cure is 90 min. at 275°F.
Shelf Life 0.333 Month
@Temperature 22.2 °C
Epoxy
 6.00 Month
@Temperature -17.8 °C
Epoxy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MTM® 49-3 Epoxy Prepreg with 36% M46J-124 Carbon Fiber
Solvay CYCOM® 950-1 Epoxy Prepreg Unidirectional Tape with 36%-M55J-140 GSM
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
APCM DA 4518U/E-Glass Unidirectional E-Glass Epoxy Prepreg
APCM DA 409U/S2-Glass Unidirectional Epoxy Prepreg

PCYTED098 / 180400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.