MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lotus Nano Paint NAP 201 Fast Dry Nano-paint
Categories: Fluid

Material Notes: Description: In some traffic marking it isn’t possible for us to close roads for long time because of traffic conditions. This paint dry fast and we can reduce the closing time of the road or avoid closing the roads.

Applications: Highway and inter-city roads

Information provided by Lotus Nanopaint

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 - 1.60 g/cc1.50 - 1.60 g/ccASTM D1475
Solids Content 50 - 54 %50 - 54 %by Volume
 71 - 75 %71 - 75 %by Weight; ASTM D1644
 
Processing PropertiesMetricEnglishComments
Dry Time 0.167 hour
@Temperature 25.0 °C
0.167 hour
@Temperature 77.0 °F
ASTM D711
 
Descriptive Properties
ColorWhite and YellowASTM EN 1439
Coverage7.9 m2/LiterASTM D344
CuringSolvent Evaporation
Direction Reflectance (%)~55%Colored, ASTM E97
 87White, ASTM E97
GlossOpaque
ResinAcrylic
Skiing Resistance (SRT)PassesASTM EN 1436
ThinnerLotus 65 B
Water ResistancePassesASTM D870

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTATP10 / 135228

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.