MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Nickel Alloy 59, UNS N06059
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: This alloy is noted for its resistance to a wide range of corrosive environments, both oxidizing and reducing.

This alloy was developed by ThyssenKrupp VDM.

Key Words: Nicrofer® 59
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.60 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 690 MPa100000 psisheet and strip 0.5 to 6.4 mm
 690 MPa
@Thickness 5.00 - 30.0 mm
100000 psi
@Thickness 0.197 - 1.18 in
plate
 650 MPa
@Diameter >=100 mm
94300 psi
@Diameter >=3.94 in
rod, bar, forgings
 690 MPa
@Diameter <=100 mm
100000 psi
@Diameter <=3.94 in
rod, bar, forgings
Tensile Strength, Yield  320 MPa
@Strain 0.2 %
46400 psi
@Strain 0.2 %
rod, bar, forgings > 100 mm
 340 MPa
@Strain 0.2 %
49300 psi
@Strain 0.2 %
sheet and strip 0.5 to 6.4 mm
 340 MPa
@Strain 0.2 %
49300 psi
@Strain 0.2 %
rod, bar, forgings < 100 mm
 340 MPa
@Strain 0.2 %,
Thickness 5.00 - 30.0 mm
49300 psi
@Strain 0.2 %,
Thickness 0.197 - 1.18 in
plate
 380 MPa
@Strain 1 %,
Thickness 5.00 - 30.0 mm
55100 psi
@Strain 1 %,
Thickness 0.197 - 1.18 in
plate
 380 MPa
@Strain 1 %,
Thickness 0.500 - 6.40 mm
55100 psi
@Strain 1 %,
Thickness 0.0197 - 0.252 in
sheet and strip
 360 MPa
@Diameter >=100 mm,
Strain 1 %
52200 psi
@Diameter >=3.94 in,
Strain 1 %
rod, bar, forgings
 380 MPa
@Diameter <=100 mm,
Strain 1 %
55100 psi
@Diameter <=3.94 in,
Strain 1 %
rod, bar, forgings
Elongation at Break 40 %40 %A5; 5.0 to 30 mm plate
 40 %40 %A5; rod, bar, forgings > 100 mm
 40 %40 %A5; sheet and strip 0.5 to 6.4 mm
 40 %40 %A5; rod, bar, forgings < 100 mm
Modulus of Elasticity 210 GPa30500 ksi
Impact >= 225>= 225J/cm² for ISO V-notch impact toughness
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000126 ohm-cm0.000126 ohm-cm
Magnetic Permeability <= 1.001
@Temperature 20.0 °C
<= 1.001
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.9 µm/m-°C
@Temperature 20.0 - 100 °C
6.61 µin/in-°F
@Temperature 68.0 - 212 °F
 12.2 µm/m-°C
@Temperature 20.0 - 200 °C
6.78 µin/in-°F
@Temperature 68.0 - 392 °F
 12.5 µm/m-°C
@Temperature 20.0 - 300 °C
6.94 µin/in-°F
@Temperature 68.0 - 572 °F
 12.7 µm/m-°C
@Temperature 20.0 - 400 °C
7.06 µin/in-°F
@Temperature 68.0 - 752 °F
 12.9 µm/m-°C
@Temperature 20.0 - 500 °C
7.17 µin/in-°F
@Temperature 68.0 - 932 °F
 13.1 µm/m-°C
@Temperature 20.0 - 600 °C
7.28 µin/in-°F
@Temperature 68.0 - 1110 °F
Specific Heat Capacity 0.414 J/g-°C0.0989 BTU/lb-°F
Thermal Conductivity 10.4 W/m-K72.2 BTU-in/hr-ft²-°F
Melting Point 1310 - 1360 °C2390 - 2480 °F
Solidus 1310 °C2390 °F
Liquidus 1360 °C2480 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 1100 - 1180 °C2010 - 2160 °F1120°C is preferred
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.10 - 0.40 %0.10 - 0.40 %
Carbon, C <= 0.010 %<= 0.010 %
Chromium, Cr 22 - 24 %22 - 24 %
Cobalt, Co <= 0.30 %<= 0.30 %
Iron, Fe <= 1.5 %<= 1.5 %
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo 15 - 16.5 %15 - 16.5 %
Nickel, Ni 56 - 63 %56 - 63 %As Remainder
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S <= 0.0050 %<= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Sandvik Sanicro 59 Covered electrodes
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C)
Aluminum 2024-T6
AISI Type 316L Stainless Steel, annealed sheet

NTHYSS000 / 19277

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.