MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load bearing property but need to be flexible. The firmness of this material is similar to that of microcellular foams, but it is lighter than microcellular foams. This material may also be suitable for some bumper or vibration dampening parts.

The components are liquid at room temperature. It has relatively long pot life (40 – 45 seconds) for a flexible foam material, so it is easier to handle by a manual hand-mixing method. This material can be open-cast into a slab for farther fabrication or molded in a compression mold. The free-rise density of the foam is 8 pounds per cubic foot, and the cell structure is open-cell.

The isocyanate component for this formulation is MDI, which is generally considered safer than TDI. This formulation does not use auxiliary blowing agent such as Freon, HCFC, CFC, or flammable hydrocarbon materials. Only normal handling for typical industrial chemicals is required. Relatively safe and easy handling and the physical properties of this foam satisfy the requirements for a variety of custom applications.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.136 g/cc0.00492 lb/in³Free Rise Density
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 35 - 4035 - 40
Tensile Strength 0.414 MPa60.0 psi
Elongation at Break 40 %40 %
Rebound 22 %22 %Bashore Rebound
Tear Strength 0.877 kN/m5.00 pliSplit
 4.73 kN/m27.0 pliDie-C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 - 32.2 °C70.0 - 90.0 °FPrepolymer Temperature
 21.1 - 32.2 °C70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 37.8 - 43.3 °C100 - 110 °F
Cure Time  30.0 - 40.2 min
@Temperature 43.3 °C
0.500 - 0.670 hour
@Temperature 110 °F
De-mold Time
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Complete Cure Cycle
Pot Life 0.670 min0.670 min
 
Descriptive Properties
Curing AgentPLE-016
Mixing Time20-25for manual hand-mix
PrepolymerMSA-018
Weight Ratio1:0.86Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
Covestro Bayfit® 566 Polyurethane Flexible Foam System, 100 Index
Covestro Bayfit® SA512 Flexible Polyurethane Foam, 75 Index
Covestro Bayfit® SA513 Flexible Polyurethane Foam, 95 Index
Overview of materials for Polyester Film

PNORTH899 / 162615

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.