Lustran® 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran ABS virgin and regrind materials to optimize cost and performance. Features: Medium flow, Medium Impact strength, Low gloss, Low gel. Applications: Used as a blending grade for extrusion applicationsInformation provided by Styrolution. |