Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAKEEP® Care M33 G HP PEEK, Medical Device Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® Care-grades are ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care M33 G-HP is a mediumviscosity, unreinforced polyether ether ketone for injection molding and extrusion. The product is refined by Evonik’s special filtration technology. The semi-crystalline polymer features superior thermal and chemical resistance. Parts made from VESTAKEEP® Care M33G-HP are of low flammability. VESTAKEEP® Care M33 G-HP can be processed by common machines for thermoplastics.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Opaque
Resistance to: Heat (thermal stability), Fire / burn
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Special Characteristics: Semi-crystalline, Medium viscosity
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00900 cm/cm0.00900 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cm0.0110 in/inISO 294-4, 2577
Melt Flow 20.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
20.0 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 98.0 MPa14200 psiISO 527
Elongation at Break 25.0 %25.0 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 3.60 GPa522 ksiISO 527
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cm?V; IEC 62631-3-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
IEC 60695-11-10
Glow Wire Ignition Temperature 800 °C
@Thickness 3.20 mm
1470 °F
@Thickness 0.126 in
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 180 °C356 °F
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7843 / 324975

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.