MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Meehanite GM-60 Flake Graphite Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a very fine finish and is recommended for heavy section casting where pressure tightness is required.

General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.

Information provided by Meehanite Marketing Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.34 g/cc7.34 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 230230Nominal
Tensile Strength, Ultimate 414 MPa60000 psi
Tensile Strength, Yield 172 MPa25000 psi.01% permanent set
Modulus of Elasticity 148 GPa21500 ksi
Modulus of Rupture 0.641 GPa93.0 ksi
Compressive Strength 1380 MPa200000 psi
Poissons Ratio 0.330.33
Fatigue Strength 172 MPa25000 psi
Machinability 50 %50 %Dalcher
Shear Modulus 65.5 GPa9500 ksi
Shear Strength 365 MPa53000 psi
Izod Impact Unnotched 40.7 - 54.2 J
@Diameter 20.3 mm
30.0 - 40.0 ft-lb
@Diameter 0.798 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.7 µm/m-°C
@Temperature 37.8 - 538 °C
7.05 µin/in-°F
@Temperature 100 - 1000 °F
Thermal Conductivity 51.2 W/m-K
@Temperature 10.0 - 232 °C
355 BTU-in/hr-ft²-°F
@Temperature 50.0 - 450 °F
Shrinkage 1.3 - 1.5 %1.3 - 1.5 %Patternmaker Shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Meehanite AQ Flake Graphite Cast Iron
Meehanite GC-40 Flake Graphite Cast Iron
SAE J431 automotive gray cast iron, SAE grade G1800
Gray Cast Iron, ASTM A 48 Class 40
Meehanite GA-50 Flake Graphite Cast Iron

NMEE01 / 18222

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.