MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals ARCEL® 207 Expanded Polyethylene/Styrenic Polymer
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: ARCEL® advanced foam resins provide solutions to a multitude of packaging and product challenges. ARCEL resins meet the needs for protective packaging, protective material handling, safety, automotive, recreational, and other applications. When used for protective packaging and material handling, ARCEL resin is a sustainable solution that reduces packaging size and weight, while maintaining superb protective properties. In comparison to traditional foam packaging, ARCEL resin reduces package size by as much as 40%.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 - 1.00 g/cc0.960 - 1.00 g/cc
Density >= 0.0120 g/cc>= 0.000434 lb/in³Continuous Double Pass Expansion (Pre-Puff)
 >= 0.0151 g/cc>= 0.000546 lb/in³Batch Single Pass Expansion (Pre-Puff)
 >= 0.0160 g/cc>= 0.000578 lb/in³Continuous Single Pass Expansion (Pre-Puff)
Volatiles 0.30 %0.30 %Plasticizer, average
 7.5 %7.5 %Pentane, average
Bead Size <= 2.40 mm<= 0.0945 in< 10% frequency
 2.00 - 3.50 mm0.0787 - 0.138 in> 98% frequency
 >= 3.40 mm>= 0.134 in< 16% frequency
 
Descriptive Properties
Colorwhite
ShapeSpherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOV617 / 249064

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.