Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids. Available in: North America Product Applications: TECHNYL® AR 218 V33 BLACK 34N is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as: - cooling and heating radiator systems, header tanks, thermostat components, inlet/outlet pipes. This product is available in black. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |