MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chengdu Letain ZW-3208 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Resin of LTP ZW-3200 serials is crystal whisker reinforced composite materials based on Polyformaldehyde. With the characteristics of outstanding thermal stability, self-lubricating and frost resisting, the materials can be used long time about 20? lower than the Temperature of thermal deformation without any lubrication additive. And it is the first choice for parts of rolling and sliding machine. Compare to Polyformaldehyde, Resin of LTP ZW-3200 serials have good mold technology without irritating smell and its products are according with RoHS index.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³GB1033
Water Absorption 0.20 %0.20 %GB1034
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in80×80×3.0
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/in80×80×3.0
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psiGB/T1040
Elongation at Break 1.2 - 2.5 %1.2 - 2.5 %GB/T1040
Flexural Strength 90.0 MPa13100 psiGB/T1042
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²GB/T1043
 
Descriptive Properties
Friction factor0.10-0.15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT034 / 255887

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.