MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Grade 704 Zirconium (Zr-1.5Sn)
Categories: Metal; Nonferrous Metal; Zirconium Alloy

Material Notes: Characteristics:
  • Contains halfnium
  • Mechanical Properties similar to pure zirconium, stronger and less ductile
  • Excellent corrosion resistance
  • Forms a stable, dense, self-healing oxide layer
  • Highly anisotropic

Applications: Chemical processing equipment

Machining Parameters: Use slow speeds, heavy feeds and flood cooling with a water-soluble oil lubricant.

Key Words: UNS R60704, Zircadyne® 704
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 6.56 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 413 MPa
 220 MPa
@Temperature 400 °C
 260 MPa
@Temperature 300 °C
 360 MPa
@Temperature 200 °C
 480 MPa
@Temperature 100 °C
 530 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 120 MPa
@Temperature 400 °C
 140 MPa
@Temperature 300 °C
 190 MPa
@Temperature 200 °C
 280 MPa
@Temperature 100 °C
 360 MPa
@Temperature 20.0 °C
 >= 241 MPa
@Strain 0.2 %
Elongation at Break 14 %in 50 mm
 22 %
@Temperature 20.0 °C
 26 %
@Temperature 100 °C
 32 %
@Temperature 200 °C
 34 %
@Temperature 400 °C
 38 %
@Temperature 310 °C
Modulus of Elasticity 99.3 GPa
Poissons Ratio 0.37
Shear Modulus 36.2 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µm/m-°C
@Temperature 25.0 °C
Specific Heat Capacity 0.285 J/g-°C
Thermal Conductivity 21.5 W/m-K
Melting Point 1850 °C
Boiling Point 4375 °C
 
Component Elements PropertiesOriginal ValueComments
Fe + Cr 0.30 %
Hafnium, Hf <= 4.5 %
Oxygen, O 0.18 %
Tin, Sn 1.5 %
Zirconium, Zr >= 97.5 %includes Hf
 
Descriptive Properties
Alpha Phase Crystal Structurehcp< 865°C
Beta Phase Crystal Structurebcc> 865°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zirconium Oxide, Zirconia, ZrO2
Zircaloy-2 Zirconium Alloy
Zircaloy-4 Zirconium Alloy
Grade 702 Zirconium, Commercially Pure
Assab Steels 8407 SUPREME Hot Work Steel

MZRI10 / 14571

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.