MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Precision Polymer Engineering N80L Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nitrile Butadiene Rubber, 75-85 °IRHD. Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000 line call-out M6BG814, A14, B14, EO14, EO34, F17.

Applications: The low acrylonitrile content of this compound provides excellent low temperature flexibility, in sealing conditions where resistance to mineral oil, alcohol, paraffin and low-aromatic petrol is required. Not recommended for use with acetone, benzene, chlorinated solvents or high-aromatic petrol. Good water resistance but poor against ozone and weather.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080°IRHD; ASTM D1415
 8585°IRHD, +5 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa1160 psi-20% change after 70 hours @ 100°C; ASTM D412
 10.0 MPa1450 psiASTM D412
Elongation at Break 100 %100 %-20% change after 70 hours @ 100°C; ASTM D412
 125 %125 %ASTM D412
Compression Set 30 %
@Temperature 100 °C,
Time 86400 sec
30 %
@Temperature 212 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 -40.0 °C-40.0 °FNon-brittle after 3 minutes
Flash Point >= 300 °C>= 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRECI201 / 57925

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.