MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Thermalux® Film Made from UDEL® Polysulfone Resin
Categories: Polymer; Film; Thermoplastic; Polysulfone (PSU)

Material Notes: Exceptional electrical properties over varying conditions. Excellent mechanical properties. Good chemical resistance. Hydrolytically stable. Transparency. FDA compliant.

Udel® is a trade name of Solvay Advanced Polymers. Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.30 %ASTM D570; 24 hrs.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10600 psiASTM D882
Elongation at Break 110 %ASTM D882
Tensile Modulus 360000 psiASTM D882
Flexural Modulus 390000 psiASTM D790
Tear Strength 6.30 kg(f)/cmASTM D1004
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 3.00e+16 ohmASTM D257
Dielectric Constant 3.14
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 2400 V/mil
@Thickness 0.102 mm
ASTM D149
Dissipation Factor 0.0013
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 302 °FContinuous Use
Deflection Temperature at 1.8 MPa (264 psi) 345 °FASTM D648
Glass Transition Temp, Tg 190 °CASTM D3418
Flammability, UL94 HB
Oxygen Index 30 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.633
Haze 0.60 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polysulfone (PSU)
Syensqo (Solvay Specialty Polymers) Udel® P-3700 HC Polysulfone (PSU)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
BASF Ultrason® S 3010 PSU
Isoflon PSU Polysulfone

PWEST083 / 72742

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.