MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) SILCOLAPSE® 422 Silicone Emulsion
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE® 422 is a 10% active silicone defoamer, which is very effective in the prevention, control or suppression of foam produced in aqueous media. It is designed for industrial use only.

Applications: SILCOLAPSE® Antifoam 422 can be used in various sectors of the industry such as:

  • Rubber: Synthetic rubber processing, synthetic latex processing
  • Chemical Processes: Manufacture of agriculture chemicals (weed killers, insecticides, fungicides...); Manufacture of adhesives and glues; Manufacture of soaps and industrial detergents; Additives for cutting oils
  • Paints, Inks and Varnishes: manufacture, packaging.
  • Textiles: Conventional dyeing, high temperature dyeing, printing, finishing, desizing of fibers, washing.
Features:
  • Disperses very easily in aqueous media
  • In dilution is homogeneous and stable in time
  • Very effective as an anti-foaming agent in a many applications

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
pH 5.55.5
Storage Temperature 1.00 - 25.0 °C33.8 - 77.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
Appearancewhite to white gray, homogeneous milky liquid
Content10% Active
Diluentswater
Effective Concentrations10-1000 ppm
Emulsifier typenonionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Dehesive® 919 Silicone Release Coating
Wacker Belsil® DM 0.65 Disiloxane
Honeywell Solstice® 1233zd(E) Blowing Agent
Elkem (Bluestar Silicones) BLUESIL™ EMUL E1P Silicone Emulsion -Release Agent

PBLUST016 / 190992

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.