MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes:

Characteristics:

  • Excellent Dimensional properties
  • Transparent
  • Improved Impact Strength and Toughness as compared to PES
  • Excellent Hydorlytic Stability
  • High Stress Cracking Resistance
  • Good Chemical Resistance
  • Good Surface Release properties
  • Tg of 224°C
  • Expected Continuous Temperature of 180°C

Applications:

  • Food
  • Contact
  • Medical
  • Electrical and Electronics
  • Auto

Information provided by Gharda Chemicals

Solvay Advanced Polymers completed its acquisition of this product line in May 2006.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Water Absorption 0.53 %24 Hours; ASTM D570
Melt Flow 13.4 - 26.8 g/10 min
@Load 2.16 kg,
Temperature 380 °C
6`; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 90.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Tensile Modulus 2.70 GPaASTM D638
Flexural Strength 120 MPaASTM D790
Flexural Modulus 2.70 GPaASTM D790
Izod Impact, Notched 75.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant 3.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.0 kV/mmASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 50 secASTM D495
Comparative Tracking Index 150 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 51.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Maximum Service Temperature, Air 180 °C
Deflection Temperature at 1.8 MPa (264 psi) 198 °CASTM D648
Glass Transition Temp, Tg 225 °CASTM D3482
Flammability, UL94 V-0
@Thickness 0.900 mm
UL 94
Oxygen Index 39 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® PF-1000 Polysulfone
Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod
Gharda Chemicals Gafone™ T6300 Polysupersulfone (PSS)
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)

PGHARDA31 / 41804

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.