Physical Properties | Metric | English | Comments |
---|
Density | 1.57 g/cc | 0.0567 lb/in³ |
Water Absorption | 4.0 % @Thickness 2.00 mm | 4.0 % @Thickness 0.0787 in |
Moisture Absorption | 1.10 % @Thickness 2.00 mm | 1.10 % @Thickness 0.0787 in |
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in |
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 220 MPa | 31900 psi |
Tensile Stress | 50.0 MPa @Strain 2 %, Temperature 140 °C | 7250 psi @Strain 2 %, Temperature 284 °F |
| 90.0 MPa @Strain 6.0 %, Temperature 140 °C | 13100 psi @Strain 6.0 %, Temperature 284 °F |
| 100 MPa @Strain 0.5 %, Temperature 23.0 °C | 14500 psi @Strain 0.5 %, Temperature 73.4 °F |
| 100 MPa @Strain 1 %, Temperature 60.0 °C | 14500 psi @Strain 1 %, Temperature 140 °F |
| 100 MPa @Strain 1.9 %, Temperature 90.0 °C | 14500 psi @Strain 1.9 %, Temperature 194 °F |
| 100 MPa @Strain 4 %, Temperature 120 °C | 14500 psi @Strain 4 %, Temperature 248 °F |
| 110 MPa @Strain 6.0 %, Temperature 120 °C | 16000 psi @Strain 6.0 %, Temperature 248 °F |
| 125 MPa @Strain 5.0 %, Temperature 90.0 °C | 18100 psi @Strain 5.0 %, Temperature 194 °F |
| 175 MPa @Strain 4 %, Temperature 60.0 °C | 25400 psi @Strain 4 %, Temperature 140 °F |
| 200 MPa @Strain 2 %, Temperature 23.0 °C | 29000 psi @Strain 2 %, Temperature 73.4 °F |
Elongation at Break | 2.7 % | 2.7 % |
Tensile Modulus | 16.5 GPa | 2390 ksi |
Flexural Strength | 340 MPa | 49300 psi |
Flexural Modulus | 14.9 GPa | 2160 ksi |
Secant Modulus | 2.00 GPa @Strain 6.0 %, Temperature 120 °C | 290 ksi @Strain 6.0 %, Temperature 248 °F |
| 2.00 GPa @Strain 8.0 %, Temperature 140 °C | 290 ksi @Strain 8.0 %, Temperature 284 °F |
| 2.50 GPa @Strain 5.5 %, Temperature 90.0 °C | 363 ksi @Strain 5.5 %, Temperature 194 °F |
| 2.50 GPa @Strain 4 %, Temperature 120 °C | 363 ksi @Strain 4 %, Temperature 248 °F |
| 2.50 GPa @Strain 4 %, Temperature 140 °C | 363 ksi @Strain 4 %, Temperature 284 °F |
| 4.00 GPa @Strain 0.0 %, Temperature 140 °C | 580 ksi @Strain 0.0 %, Temperature 284 °F |
| 5.00 GPa @Strain 2.1 %, Temperature 90.0 °C | 725 ksi @Strain 2.1 %, Temperature 194 °F |
| 5.00 GPa @Strain 3.2 %, Temperature 60.0 °C | 725 ksi @Strain 3.2 %, Temperature 140 °F |
| 5.50 GPa @Strain 0.0 %, Temperature 120 °C | 798 ksi @Strain 0.0 %, Temperature 248 °F |
| 7.25 GPa @Strain 2 %, Temperature 60.0 °C | 1050 ksi @Strain 2 %, Temperature 140 °F |
| 9.50 GPa @Strain 0.0 %, Temperature 90.0 °C | 1380 ksi @Strain 0.0 %, Temperature 194 °F |
| 10.0 GPa @Strain 2 %, Temperature 23.0 °C | 1450 ksi @Strain 2 %, Temperature 73.4 °F |
| 16.0 GPa @Strain 0.0 %, Temperature 23.0 °C | 2320 ksi @Strain 0.0 %, Temperature 73.4 °F |
| 17.5 GPa @Strain 0.0 %, Temperature 60.0 °C | 2540 ksi @Strain 0.0 %, Temperature 140 °F |
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² |
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm |
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm |
|
Thermal Properties | Metric | English | Comments |
---|
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F |
Vicat Softening Point | 255 °C @Load 5.10 kg | 491 °F @Load 11.2 lb |
Flammability, UL94 | HB @Thickness 0.800 mm | HB @Thickness 0.0315 in |
Flame Spread | 0.000 mm/min @Thickness 3.00 mm | 0.000 in/min @Thickness 0.118 in |
Glow Wire Flammability Index | 700 °C @Thickness 2.00 mm | 1290 °F @Thickness 0.0787 in |
|
Processing Properties | Metric | English | Comments |
---|
Melt Temperature | 280 - 300 °C | 536 - 572 °F |
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.