MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Redwood Plastics TIVAR® DRYSLIDE UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Ideal for dusty environments, Redco™ Tivar® Dryslide is electro static dissipative which eliminates shock due to friction. Redco™ Tivar® Dryslide is also corrosion-resistant, self-lubricating (dry lubricant formulation) with no moisture absorption.

Standard Color: Blue, White & Black

Fusion welded Redco™ UHMW sheets are available to eliminate lifting; up to 144” x 1200”.

Typical Applications: Belt skirting, chute liners, conveying components, bearings, belt guides, chain guides, curves, guide rails, wear strip, dead plates, diverter bars, guide rollers, hitch plates, hopper liners, liners for gravity flow applications, roller covers, transfer plates, under belt wear strips, belt scrapers, bunker liners, chain conveyor flights, chute liners, conveyor skirting, cyclones, drag chain conveyor liners, dragline buckets, dust collection hopper liners, front end loader bucket liners, hopper liners, off-road truck beds, truck bed lining for asphalt hauling, pugmill paddles, railcar liners, reclaimer buckets, screw conveyor liners, self-unloading ships, silo liners, slider beds, storage bin liners surge bin liners, transfer chute liners, under chain guides, vibrating bin, dischargers, vibratory feeder liners, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ASTM D 2240
Tensile Strength at Break 33.20 MPa4815 psiASTM D638
Tensile Strength, Yield 19.1 MPa2770 psiASTM D638
Elongation at Break 200 %200 %ASTM D 638
Tensile Modulus 0.818015 GPa118.643 ksiASTM D638
1% Secant Modulus 734.009 MPa106459 psiASTM D790B
Izod Impact, Notched NBNBASTM D256A
Tensile Impact Strength 1370 kJ/m²653 ft-lb/in²ASTM D1822
Coefficient of Friction, Dynamic 0.0800.080(DRY vs. STEEL)
Coefficient of Friction, Static 0.150.15(DRY vs. STEEL)
Abrasion 1010Sand Slurry, 1018 steel=100
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+9 ohm-cm>= 1.00e+9 ohm-cmASTM D 257
Surface Resistance 1e+05 - 1.00e+9 ohm1e+05 - 1.00e+9 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature -30.0 - 60.0 °C
11.1 µin/in-°F
@Temperature -22.0 - 140 °F
ASTM D-2240
Maximum Service Temperature, Air 82.2 °C180 °FConstant
 93.3 °C200 °FIntermittent
 
Descriptive Properties
FDA ()NO
Sand on Wheel100 mg weight lossASTM G-64

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW015 / 296581

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.