System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced, Flame Retardant
Material Notes:
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowability
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.169
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.0010
cm/cm
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
0.011
cm/cm
60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0010
cm/cm
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
0.011
cm/cm
60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
50.0
MPa
cond.; ISO 527-1, -2; 50 mm/min
85.0
MPa
d.a.m.; ISO 527-1, -2; 50 mm/min
Elongation at Yield
4.1 %
d.a.m.; ISO 527-1, -2; 50 mm/min
>= 20 %
cond.; ISO 527-1, -2; 50 mm/min
Tensile Modulus
1500
MPa
cond.; ISO 527-1, -2; 1 mm/min
3800
MPa
d.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength
55.0
MPa
@Strain 8.0 %
cond., 2 mm/min; ISO 178-A
135
MPa
@Strain 5.8 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Yield Strength
40.0
MPa
@Strain 3.5 %
cond., 2 mm/min; ISO 178-A
115
MPa
@Strain 3.5 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus
1600
MPa
cond., 2 mm/min; ISO 178-A
3900
MPa
d.a.m., 2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
d.a.m.; ISO 180-1A
<=
10.0
kJ/m²
cond.; ISO 180-1A
Izod Impact, Unnotched (ISO)
45.0
kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 180-1U
45.0
kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 180-1U
55.0
kJ/m²
@Temperature -30.0 °C
cond.; ISO 180-1U
NB
@Temperature 23.0 °C
cond.; ISO 180-1U
Charpy Impact Unnotched
50.0
kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 179-1eU
60.0
kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 179-1eU
80.0
kJ/m²
@Temperature -30.0 °C
cond.; ISO 179-1eU
NB
@Temperature 23.0 °C
cond.; ISO 179-1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
d.a.m.; ISO 179-1eA
<=
10.0
kJ/m²
cond.; ISO 179-1eA
Electrical Properties
Original Value
Comments
Comparative Tracking Index
600
V
d.a.m.; Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
80.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
Melting Point
265
°C
10°C/min; ISO 11357-1, -3
Deflection Temperature at 0.46 MPa (66 psi)
212
°C
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
80.0
°C
ISO 75-1, -2
Vicat Softening Point
230
°C
@Load 5.10 kg
120°C/hour; ISO 306
Flammability, UL94
V-0
@Thickness 0.400 mm
Oxygen Index
35 %
Method A; ISO 4589-2
Glow Wire Ignition Temperature
775
°C
@Diameter 0.400 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Diameter 0.400 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
for test specimens; ISO 294
260
-
270
°C
Mold Temperature
80.0
°C
for test specimens; ISO 294
80.0
-
100
°C
Drying Temperature
80.0
°C
Dry Time
2
-
6
hour
Moisture Content
0.030 - 0.070 %
residual; Karl Fischer Test
Descriptive Properties
ISO Short Name
ISO 1874-PA 66, GF, 14-040; ISO 1043 PA FR(30)
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Oceanchem Group Melamine Polyphosphate (MPP)
Overview of materials for Nylon 6 Fiber
Lanxess Durethan® DP A 30 S FN30 000000 Nylon 66
PLANX0644 / 133607
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.