Product Code: MSHQD -VA031-05 OT Chemical Name: Polymeric Sulfur Trade Name: Rubber Vulcanization Agent IS 75-20 CAS No.: Polymeric Sulfur: 9035-99-8; Rhombic Sulfur: 7704-34-9; High pressure and hydrotreated naphthenic oil: 64742-52-5 Typical Properties: Yellow powder with little odor, no poison. The relative density is 1.60-1.70. It is not stability, it can be reduced content and then become to soluble sulfur. Insoluble in CS2 and water. Recommended Applications: IS 75-20 is designed for improved flowability and dispersibility.it has the following advantages: Improved flowability. The improved product flowability provides easy handing, a less dusty enviroment and less tendency for product to compact. Improved dispersibility. The special additive package in IS 75-20 helps to reduce the tendency for electrostatic charge build-up and hence the formation of agglomerates which can be formed during mixing as a result of the small particle size of insoluble sulfur. Information provided by Meyors Chemical INC Limited |