MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Medalist® MD-50143 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-50143 is a clear high performance thermoplastic elastomer specifically designed for medical and healthcare applications. Medalist MD-50143 is a low hardness, low density, halogen-free grade that is suitable for extrusion or molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Good Sterilizability; Halogen Free; Low Density; Low Hardness; Low Specific Gravity

Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment

Agency Ratings: ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 100 g/10 min
@Load 2.16 kg,
Temperature 190 °C
100 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  40
@Time 15.0 sec
40
@Time 0.00417 hour
ASTM D2240
 43
@Time 5.00 sec
43
@Time 0.00139 hour
ASTM D2240
 45
@Time 1.00 sec
45
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 5.52 MPa800 psiASTM D412
Elongation at Break 680 %680 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 193 °C340 - 380 °FMelt, Injection
Rear Barrel Temperature 127 - 149 °C260 - 300 °FInjection
Middle Barrel Temperature 138 - 160 °C280 - 320 °FInjection
Front Barrel Temperature 149 - 171 °C300 - 340 °FInjection
Nozzle Temperature 171 - 193 °C340 - 380 °FInjection
Zone 1 171 - 188 °C340 - 370 °FExtrusion
Zone 2 182 - 196 °C360 - 385 °FExtrusion
Zone 3 177 - 204 °C350 - 400 °FExtrusion
Zone 4 185 - 204 °C365 - 400 °FExtrusion
Zone 5 204 - 227 °C400 - 440 °FExtrusion
Die Temperature 204 - 227 °C400 - 440 °FExtrusion
Mold Temperature 21.1 - 37.8 °C70.0 - 100 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0727 / 237218

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.