MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 76® Lubricants Triton® 680 GEO SAE Grade 30  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: 76® Triton 680 GEO is a premium quality, low-ash, dispersant detergent gas engine oil designed for use in high-output, 4-stroke cycle natural gas engines operating under heavy loads and extreme temperatures. Engines operating in this type of service typically are found on crude oil and gas transmission pipelines, electrical power generators, gas compressors, irrigation water pumps and well drilling rigs. Triton 680 GEO is formulated with field-proven performance additives to meet the rigorous lubrication demands of modern, fuel-efficient, low-emission gas engines. It provides excellent resistance to oil oxidation and nitration, protects against ring and liner wear, helps minimize engine sludge and piston deposits for outstanding engine cleanliness, and protects against corrosion. It also protects against valve stem deposits and valve recession, resulting in reduced maintenance and extended engine life. The additive package has low phosphorus content to meet the requirements of gas engines equipped with catalysts for exhaust after-treatment.

Applications:

  • Turbocharged, lean-burn and naturally aspirated 4-stroke cycle natural gas engines where the manufacturer specifies a low-ash gas engine oil meeting API CD performance requirements
Triton 680 GEO is recommended for use in natural gas engines manufactured by:
  • Caterpillar
  • Climax
  • Colt-Fairbanks Morse
  • Dresser Rand (Category I, II, III)
  • Minneapolis Moline
  • Nordberg
  • Ruston
  • Superior
  • Wartsila
  • Waukesha
  • Worthington
Features/Benefits:
  • Field-proven performance in providing outstanding engine cleanliness
  • Proven performance in lean-burn engines
  • High dispersancy protects against engine sludge and varnish deposits
  • Excellent resistance to oil oxidation and nitration
  • Protects against scuffing and wear
  • Protects against rust and corrosion
  • Protects against valve stem deposits and valve recession
  • Compatible with emissions system catalysts
  • Does not contain any bright stock, which can cause harmful carbon deposits

Information provided by Phillips 66 Lubricants. The 76® Lubricants brand name was consolidated into other Phillips 66 brands in 2016; many products remain available under a new name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.886 g/cc
Density 7.38 lb/gal
Viscosity Measurement 96Index
Kinematic Viscosity at 40°C (104°F) 94 cSt
Kinematic Viscosity at 100°C (212°F) 10.7 cSt
Ash 0.45 %Sulfated; ASTM D874
ASTM Color 6.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 4.2ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -36.0 °C
Flash Point 254 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.028 %
Zinc, Zn 0.032 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON6419 / 210055

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.