MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Eastar™ Renew GN071-15, Natural Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar™ Renew GN071-15 copolyester is a sustainable, clear copolyester used in a variety of packaging and consumer product applications, including food and beverage packaging, general-purpose packaging, flexible film packaging, and consumer products. It is among the easiest resins to extrude into thin films and rigid, thermoformed containers. Eastar™ Renew GN071-15 copolyester enables fast-moving consumer goods brand owners to reduce their consumption of plastics made from fossil feedstocks, satisfy NGO (nongovernmental organizations) and governmental requirements for sustainability, reduce their carbon footprint, and be fast movers in a growing market for sustainable consumer products. Packaging converters prefer Eastar™ Renew GN071-15 copolyester for its best-in-class processing ease, sustainability without compromise, energy efficiency, thermoformability, and versatility. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC-certified circular content by mass balance allocation. Eastar™ Renew GN071-15 copolyester may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations. This product has been GREENGUARD Indoor Air Quality Certified. The GREENGUARD Indoor Air Quality Certified mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, nonprofit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry-independent, third-party testing program for low emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the “Manufacturer” category and click search to display a list of our products.

Applications

  • Extruding
  • Graphic arts
  • Home, garden & automotive packaging
  • Mono-layer film food contact
  • Multi-layer film food contact
  • Packaging component - food contact
  • Packaging component films
  • Packaging components non food contact
  • Protective film
  • Transaction cards
  • Wood furniture
Key Attributes
  • Clear, bright, premium appearance
  • Easy to extrude
  • Easy to thermoform
  • Effective barrier properties
  • Great for blown film
  • Low greenhouse gas (GHG) emissions
  • Lower carbon footprint
  • Not a material of concern
  • PVC alternative
  • Polystyrene (PS) alternative

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.00200 - 0.00500 cm/cm
@Thickness 3.17 mm
0.00200 - 0.00500 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 29.0 MPa4210 psiISO 527
 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 48.0 MPa6960 psiISO 527
 50.0 MPa7250 psiASTM D638
Elongation at Break 180 %180 %ASTM D638
 200 %200 %ISO 527
Elongation at Yield 4.00 %4.00 %ISO 527
 4.40 %4.40 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiISO 527
 2.03 GPa294 ksiASTM D638
Flexural Strength 67.0 MPa9720 psiASTM D790
 68.0 MPa9860 psiISO 178
Flexural Modulus 2.06 GPa299 ksiASTM D790
Izod Impact, Notched  0.400 J/cm
@Temperature -40.0 °C
0.749 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 1.05 J/cm
@Temperature 23.0 °C
1.97 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Izod Impact, Notched (ISO)  4.50 kJ/m²
@Temperature -40.0 °C
2.14 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 9.40 kJ/m²
@Temperature 23.0 °C
4.47 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 0.200 %0.200 %ASTM D1003
Transmission, Visible 90.0 %90.0 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 63.0 °C145 °F
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hour
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4128 / 323751

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.