MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resin

Characteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248; 11 MPa Hydrostatic Design Basis at 23°C and 5.5 MPa Hydrostatic Design Basis at 60°C

Applications: potable water, industrial and mining, oil and gas gathering

PENT is 150 hours per ASTM F 1473.

Information provided by Chevron Phillips Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
Conditions A, B and C; ASTM D 1693
Melt Flow 0.11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.11 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 34.0 MPa4930 psiASTM D638 Type IV
Tensile Strength, Yield 22.0 MPa3190 psiASTM D638 Type IV
Elongation at Break >= 500 %>= 500 %ASTM D638 Type IV
Flexural Modulus 0.960 GPa139 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -90.0 °C<= -130 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 216 °C379 - 421 °Fadequate mixing to achieve good dispersion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Autoclaved aerated concrete, 0.500 g/cc density
Asphalt
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete
Concrete, 1-4 Dry
Concrete, foamed blast furnace slag aggregate

PCHEVM09 / 20300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.