MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Osmium, Os; Arc-Melted
Categories: Metal; Nonferrous Metal; Precious Metal; Pure Element

Material Notes: Arc-melted applies only to tensile and/or hardness values; other property values are typical of the element.

Physical Form: Blue-White Metal; Hexagonal

See entries for annealed and cold worked Os.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 22.5 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 190.231995
Atomic Number 76
Thermal Neutron Cross Section 15 barns/atom
X-ray Absorption Edge 0.1678 ÅK
 0.95574 ÅLI
 1.00129 ÅLII
 1.14143 ÅLIII
Electrode Potential 0.70 V
Electronegativity 2.2Pauling
Ionic Radius 0.690 ÅCrystal Ionic Radius for Valence +6
 0.880 ÅCrystal Ionic Radius for Valence +4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 722Converted from Vickers for 3000 kg load/10 mm ball Brinell test.
Hardness, Knoop 822Converted from Vickers.
Hardness, Rockwell A 83.4Converted from Vickers.
Hardness, Rockwell C 64Converted from Vickers.
Hardness, Vickers 800
Modulus of Elasticity 560 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000812 ohm-cm
Magnetic Susceptibility 4.0e-8cgs/g
Critical Magnetic Field Strength, Oersted 70
Critical Superconducting Temperature 0.630 - 0.690 K
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 26.8 J/g
Heat of Vaporization 678 J/g
CTE, linear 6.60 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.109 J/g-°CGas
 0.131 J/g-°C
Thermal Conductivity 91.67 W/m-K
Melting Point 3050 °C
Boiling Point 5012 °C
Heat of Formation 0.000 kJ/molCrystal
 791 kJ/molGas
 
Component Elements PropertiesOriginal ValueComments
Osmium, Os 100 %
 
Descriptive Properties
SolubilitySoluble in Aqua Regia

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Osmium, Os; Annealed
Osmium, Os; Cold-Worked
Silver, Ag
Americium, Am
Aluminum, Al

AMEOs02 / 78

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.