MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ THERMOCOMP™ Compound RF00CSXZ Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP THERMOCOMP RF00CSXZ compound is based on Nylon 6/6 resin containing 60% glass fiber. Added features of this grade include: Heat Stabilized.

Features: High Stiffness,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 g/cc0.0621 lb/in³ASTM D792
 1.72 g/cc0.0621 lb/in³ISO 1183
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.300 %0.300 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0029 cm/cm0.0029 in/in24hrs; ISO 294
 0.0030 cm/cm0.0030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
 0.0044 cm/cm0.0044 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 253 MPa36700 psiASTM D638
 253 MPa36700 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
 2.2 %2.2 %ASTM D638
Tensile Modulus 21.36 GPa3098 ksi1 mm/min; ISO 527
 21.37 GPa3099 ksi50 mm/min; ASTM D638
Flexural Strength 358 MPa51900 psiASTM D790
 375 MPa54400 psiISO 178
Flexural Modulus 19.3 GPa2800 ksiASTM D790
 20.0 GPa2900 ksiISO 178
Izod Impact Notched 160 J118 ft-lbASTM D256
Izod Impact, Unnotched 12.28 J/cm23.01 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 19.0 kJ/m²9.04 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 76.0 kJ/m²36.2 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 J7.38 ft-lbpeak; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  16.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
9.00 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 38.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  16.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
8.89 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 37.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 260 °C
@Thickness 3.20 mm
500 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C489 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 255 °C
@Thickness 3.20 mm
491 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 95.0 - 110 °C203 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81897 / 289844

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.